  "brand": "VOXFIL",
  "version": "2026.1",
  "generated": "2026-08-21",
  "note": "Import-friendly preset bundle. Values match our TDS. Tune for your printer, nozzle and environment.",
  "presets": [
    {
      "id": "pla",
      "slicer": "Recommended starting profile — tune for your printer",
      "name": "VOXFIL PLA",
      "nozzle_temp": "190 – 220 °C",
      "bed_temp": "45 – 60 °C",
      "print_speed": "60 – 150 mm/s",
      "cooling_fan": "Required (100%)",
      "retraction_hint": "Speed: up to 150 mm/s with full cooling",
      "specs_reference": "voxfil-pla.json"
    },
    {
      "id": "pla-plus",
      "slicer": "Recommended starting profile — tune for your printer",
      "name": "VOXFIL PLA+",
      "nozzle_temp": "200 – 230 °C",
      "bed_temp": "50 – 65 °C",
      "print_speed": "60 – 140 mm/s",
      "cooling_fan": "Required (100%)",
      "retraction_hint": "Speed: up to 140 mm/s, full cooling",
      "specs_reference": "voxfil-pla-plus.json"
    },
    {
      "id": "petg",
      "slicer": "Recommended starting profile — tune for your printer",
      "name": "VOXFIL PETG",
      "nozzle_temp": "230 – 250 °C",
      "bed_temp": "70 – 85 °C",
      "print_speed": "40 – 90 mm/s",
      "cooling_fan": "Low (20 – 40%)",
      "retraction_hint": "Speed: 40 – 90 mm/s, low cooling",
      "specs_reference": "voxfil-petg.json"
    },
    {
      "id": "abs",
      "slicer": "Recommended starting profile — tune for your printer",
      "name": "VOXFIL ABS",
      "nozzle_temp": "230 – 260 °C",
      "bed_temp": "90 – 110 °C",
      "print_speed": "40 – 80 mm/s",
      "cooling_fan": "Off or minimal (0 – 20%)",
      "retraction_hint": "Speed: 40 – 80 mm/s, cooling fan off",
      "specs_reference": "voxfil-abs.json"
    },
    {
      "id": "asa",
      "slicer": "Recommended starting profile — tune for your printer",
      "name": "VOXFIL ASA",
      "nozzle_temp": "240 – 260 °C",
      "bed_temp": "95 – 110 °C",
      "print_speed": "40 – 80 mm/s",
      "cooling_fan": "Off or minimal (0 – 20%)",
      "retraction_hint": "Speed: 40 – 80 mm/s, cooling off",
      "specs_reference": "voxfil-asa.json"
    },
    {
      "id": "pa",
      "slicer": "Recommended starting profile — tune for your printer",
      "name": "VOXFIL PA",
      "nozzle_temp": "250 – 270 °C",
      "bed_temp": "60 – 80 °C",
      "print_speed": "30 – 60 mm/s",
      "cooling_fan": "Low (10 – 30%)",
      "retraction_hint": "Speed: 30 – 60 mm/s, low cooling",
      "specs_reference": "voxfil-pa.json"
    },
    {
      "id": "pa-cf",
      "slicer": "Recommended starting profile — tune for your printer",
      "name": "VOXFIL PA-CF",
      "nozzle_temp": "260 – 290 °C",
      "bed_temp": "70 – 90 °C",
      "print_speed": "30 – 60 mm/s",
      "cooling_fan": "Low (10 – 30%)",
      "retraction_hint": "Speed: 30 – 60 mm/s",
      "specs_reference": "voxfil-pa-cf.json"
    },
    {
      "id": "pc",
      "slicer": "Recommended starting profile — tune for your printer",
      "name": "VOXFIL PC",
      "nozzle_temp": "260 – 300 °C",
      "bed_temp": "100 – 120 °C",
      "print_speed": "30 – 60 mm/s",
      "cooling_fan": "Off (0 – 10%)",
      "retraction_hint": "Speed: 30 – 60 mm/s, cooling off",
      "specs_reference": "voxfil-pc.json"
    },
    {
      "id": "tpu",
      "slicer": "Recommended starting profile — tune for your printer",
      "name": "VOXFIL TPU",
      "nozzle_temp": "220 – 250 °C",
      "bed_temp": "40 – 60 °C",
      "print_speed": "15 – 40 mm/s (direct drive)",
      "cooling_fan": "Low (20 – 40%)",
      "retraction_hint": "Speed: 15 – 40 mm/s, direct-drive extruder best",
      "specs_reference": "voxfil-tpu.json"
    }
  ]
}